Uberkote™ Sn SO4 Process

Uberkote™ Sn SO4 Process is a two component bright acid stannous plating process. There are five products listed below. The two component system for ease of process can be also purchased as a one-component ready-to-use. There is also a post-plate rinse to eliminate staining and improve solderability. There is also a regenerator that precipitates stannic tin that builds up in stannous tin plating. See document section below with TDS process. In the description section below is each product-click on each product for more detail information such as; SDS, package sizes, and pricing.

Out of Stock.

Uberkote™ Sn SO4 Process includes the following products:
UberkokeTM Brightener is the brightener component.
UberkoteTM  Carrier is the carrier component.
UberkoteTM RTU is the ready-to-use system that has been combined the carrier and the brightener into one component.
UberkoteTM Rinse is the post-plate rinse to eliminate staining and improve solderability.
UberkoteTM Regenerator precipitates stannic tin that builds up in tin plating. An excessive amount of stannic tin in sulphate tin
                                             plating solution can increase the additive consumption due to the organic absorbing surfaces of the
                                             colloidal surfaces.  Excessive stannic tin, in rack plating may cause roughness.   The oxidation of
                                             Stannous (Tin +2) into Stannic (Tin+4) while operating tin and tin-lead electroplating processes occurs
                                             when the stannous is exposed to oxygen. This is a natural process that can be controlled but not
                                             prevented.  The Uberkote™ Sn SO4 process contains stabilizers to slow oxidation. Combined with
                                             proper filtration will greatly reduce oxidation of the divalent tin. Avoid agitation and air in plating
                                             solution to prevent acceleration of stannic formation. If the stannic bath content increases too fast
                                             ensure the anode current density is below 15-amps/sq.ft.